[1]刘 杰, 潘晴川, 车 畅, 等. Si含量对铁基高温合金抗氧化性能的影响[J]. 铸造技术, 2017, 38(7): 1547-1550. Liu Jie, Pan Qingchuan, Che Chang, et al. Effect of Si content on oxidation resistance of iron-based superalloy[J]. Foundry Technology, 2017, 38(7): 1547-1550. [2]陈 晨, 杨志南, 张福成. 40CrNiMoV钢在大尺寸轴承中的应用[J]. 金属热处理, 2017, 42(4): 6-11. Chen Chen, Yang Zhinan, Zhang Fucheng. Application of 40CrNiMoV steel to heavy section bearing[J]. Heat Treatment of Metals, 2017, 42(4): 6-11. [3]肖逸锋, 周年丰, 吴 靓, 等. Cr含量对WC钢结硬质合金组织及力学性能的影响[J]. 金属热处理, 2017, 42(4): 22-26. Xiao Yifeng, Zhou Nianfeng, Wu Liang, et al. Effect of chromium content on microstructure and mechanical properties of WC steel bonded carbide[J]. Heat Treatment of Metals, 2017, 42(4): 22-26. [4]Pan T J, Li Y S, Yang Q, et al. Internal oxidation and phase transformations of multi-phase Fe-Ni-Al and Fe-Ni-Al-Cr alloys induced by KCl corrosion[J]. Corrosion Science, 2011, 53(6): 2115-2121. [5]王志武, 刘倩倩, 龚雪婷. Fe-Ni合金在600 ℃空气中的氧化行为[J]. 金属热处理, 2016, 41(8) : 6-10. Wang Zhiwu, Liu Qianqian, Gong Xueting. High-temperature oxidation behavior of Fe-Ni alloy at 600 ℃ in air[J]. Heat Treatment of Metals, 2016, 41(8) : 6-10. [6]Haugsrud Reidar. On the high-temperature oxidation of Fe, Co, Ni and Cu-based alloys with addition of a less noble element[J]. Materials Science and Engineering A, 2001, 298(1): 216-226. [7]陈 刚, 张 弛, 上田光敏, 等. 水蒸气对Fe-Cr-Ni合金在800 ℃时的氧化膜形貌的影响[J]. 金属热处理, 2012, 37(10): 25-28. Chen Gang, Zhang Chi, Ueda Mitsutoshi, et al. Effect of water vapor on morphology of oxide scales of Fe-Cr-Ni alloy at 800 ℃[J]. Heat Treatment of Metals, 2012, 37(10): 25-28. [8]赵 谦, 王福明, 何煜天, 等. 不同氧含量的Fe-36Ni因瓦合金的晶间内氧化行为[J]. 金属热处理, 2015, 40(11) : 60-63. Zhao Qian, Wang Fuming, He Yutian, et al. Effect of total oxygen content on intergranular oxidation behavior of Fe-36Ni invar alloy at high temperature[J]. Heat Treatment of Metals, 2015, 40(11) : 60-63. |