金属热处理 ›› 2021, Vol. 46 ›› Issue (1): 104-108.DOI: 10.13251/j.issn.0254-6051.2021.01.020

• 材料研究 • 上一篇    下一篇

新型Fe80.5Si7.2B12.3非晶合金带材的退火工艺与磁性能

宋苏1,2,3, 陈文智2, 张广强3, 郑伟1,3, 张迁1,3, 邢彦兴1,3, 周少雄2   

  1. 1.钢铁研究总院,北京 100081;
    2.安泰科技股份有限公司,北京 100081;
    3.江苏集萃安泰创明先进能源材料研究院有限公司,江苏 常州 213000
  • 收稿日期:2020-06-28 出版日期:2021-01-25 发布日期:2021-01-26
  • 通讯作者: 陈文智,高级工程师,博士,E-mail:chenwenzhi@atmcn.com
  • 作者简介:宋苏(1991—),男,硕士,主要研究方向为非晶合金的性能和工艺研究,E-mail:samuelsong815@163.com。
  • 基金资助:
    国家重点研发计划(2016YFB0300503,2017YFB0903903);新型研发机构建设(CM20177003)

Annealing process and magnetic properties of a new type Fe80.5Si7.2B12.3 amorphous alloy strip

Song Su1,2,3, Chen Wenzhi2, Zhang Guangqiang3, Zheng Wei1,3, Zhang Qian1,3, Xing Yanxing1,3, Zhou Shaoxiong2   

  1. 1. Central Iron and Steel Research Institute,Beijing 100081,China;
    2. Advanced Technology and Materials Co.,Ltd.,Beijing 100081,China;
    3. Jiangsu JITRI Advanced Energy & Materials Research Institute Co.,Ltd.,Changzhou Jiangsu 213000,China
  • Received:2020-06-28 Online:2021-01-25 Published:2021-01-26

摘要: 研究了新型Fe80.5Si7.2B12.3非晶合金带材在不同退火工艺下的磁性能及磁损耗特性,并与传统的铁基非晶合金Fe80Si9B11进行了对比。结果表明:新型Fe80.5Si7.2B12.3非晶合金带材比Fe80Si9B11具有更高的饱和磁感应强度,在励磁磁场强度为3500 A/m下其磁通密度值为1.607 T;在f=50 Hz、Bm=1.4 T下,经无磁场退火处理后其磁损耗高于Fe80Si9B11,达到0.411 W/kg;经纵磁退火后磁损耗与Fe80Si9B11基本相当,其值为0.197 W/kg;经横磁退火后损耗仅为0.175 W/kg低于Fe80Si9B11,而且初始磁导率和恒磁导率均优于Fe80Si9B11;新型Fe80.5Si7.2B12.3非晶合金带材的最佳退火温度区间(360~400 ℃)与Fe80Si9B11相当。

关键词: 高饱和磁感应强度, 非晶合金, 磁场退火, 软磁性能, 磁损耗

Abstract: Magnetic properties and loss characteristics of a new type Fe80.5Si7.2B12.3 amorphous alloy strip under different annealing processes were studied and compared with the traditional iron-based amorphous alloy Fe80Si9B11.The results indicate that the new type Fe80.5Si7.2B12.3 amorphous alloy strip has a higher saturation magnetic induction intensity than that of Fe80Si9B11,its magnetic flux density value is 1.607 T under the excitation magnetic field intensity of 3500 A/m.After annealing without magnetic field,its magnetic loss value is higher than that of Fe80Si9B11,reaching 0.411 W/kg at f=50 Hz and Bm =1.4 T.After longitudinal magnetic annealing,its magnetic loss is 0.197 W/kg and basically equivalent to that of Fe80Si9B11.After transverse magnetic annealing,its magnetic loss is only 0.175 W/kg,lower than that of Fe80Si9B11,while the initial permeability and constant permeability are better than that of Fe80Si9B11.The optimal annealing temperature range (360-400 ℃) of the new type Fe80.5Si7.2B12.3 amorphous alloy strip is equivalent to that of Fe80Si9B11.

Key words: high saturation magnetic induction, amorphous alloy, magnetic field annealing, soft magnetic property, magnetic loss