[1]屈 鹏. 航空发动机主滑油泵齿轮轴断裂分析[J]. 失效分析与预防, 2012, 7(1): 38-42. Qu Peng. Fracture analysis on gear wheel shaft of main oil pump in aero-engine[J]. Failure Analysis and Prevention, 2012, 7(1): 38-42. [2]Xu L Q, Yu X K, Hou Z G. Analysis of the causes of driving gear shaft fractures in gear pumps[J]. Journal of Failure Analysis and Prevention, 2020, 20(1): 242-248. [3]李平平, 陈凯敏, 吴建华, 等. 齿轮轴断裂原因分析及预防措施[J]. 金属热处理, 2016, 41(3): 207-209. Li Pingping, Chen Kaimin, Wu Jianhua, et al. Fracture analysis of gear shaft and preventive measures[J]. Heat Treatment of Metals, 2016, 41(3): 207-209. [4]冯志伟. CFM56-7B发动机起动机行星齿轮轴的失效分析与预防[J]. 航空维修与工程, 2020(3): 85-87. Feng Zhiwei. Failure analysis and prevention of ATS gear shaft for CFM56-7B[J]. Aviation Maintenance and Engineering, 2020(3): 85-87. [5]杨 春, 朱衍勇, 钟振前, 等. 齿轮轴纵向延迟开裂原因分析[J]. 金属热处理, 2013, 38(8): 131-134. Yang Chun, Zhu Yanyong, Zhong Zhenqian, et al. Failure analysis of longitudinal delayed cracking for gear shaft[J]. Heat Treatment of Metals, 2013, 38(8): 131-134. [6]张 兵, 石晓东, 侯 锐, 等. 齿轮轴开裂原因分析[J]. 失效分析与预防, 2022, 17(2): 124-128. Zhang Bing, Shi Xiaodong, Hou Rui, et al. Cracking cause analysis of gear shaft[J]. Failure Analysis and Prevention, 2022, 17(2): 124-128. [7]Brahimi S V, Yue S, Sriraman K R. Alloy and composition dependence of hydrogen embrittlement susceptibility in high-strength steel fasteners[J]. Philosophical Transactions of the Royal Society A, 2017, 375: 20160407-20160426. [8]张宝东, 侯 锐, 张 兵, 等. 履带限位块开裂分析[J]. 失效分析与预防, 2020, 15(4): 255-259. Zhang Baodong, Hou Rui, Zhang Bing, et al. Cracking analysis of stop blocks in caterpillar bands[J]. Failure Analysis and Prevention, 2020, 15(4): 255-259. [9]张 栋, 钟培道, 陶春虎, 等. 失效分析[M]. 北京: 国防工业出版社, 2008: 198-199. [10]Li X F, Zhang J, Ma M M, et al. Effect of shot peening on hydrogen embrittlement of high strength steel[J]. International Journal of Minerals, Metallurgy and Materials, 2016, 23(6): 667-675. [11]陈德华, 藤鲁湘, 李光瑾. 渗碳淬硬层残余应力的分布特征[J]. 热处理, 2011, 26(2): 65-71. Chen Dehua, Teng Luxiang, Li Guangjin. Distribution characteristics of residual stress in carburized and gardened case[J]. Heat Treatment, 2011, 26(2): 65-71. [12]Murakami Y, Kanezaki T, Sofronis P. Hydrogen embrittlement of high strength steels: Determination of the threshold stress intensity for small cracks nucleating at nonmetallic inclusions[J]. Engineering Fracture Mechanics, 2013, 97(1): 227-243. [13]Fujita S, Murakami Y. A new inclusion rating method by positive use of hydrogen embrittlement phenomenon[J]. Metallurgical and Materials Transactions A, 2013, 44(1): 303-322. |