[1]Ha J W, Seong B S, Jeong H W, et al. Effects of the aging temperature and stress relaxation conditions on γ′ precipitation in Inconel X-750[J]. Journal of Nuclear Materials, 2015, 457: 362-368. [2]Marsh C, Depinoy S, Kaoumi D. Effect of heat treatment on the temperature dependence of the fracture behavior of X-750 alloy[J]. Materials Science and Engineering A, 2016, 677: 474-484. [3]Hwang J Y, Banerjee R, Tiley J, et al. Nanoscale characterization of elemental partitioning between gamma and gamma prime phases in René 88 DT nickel-base superalloy[J]. Metallurgical and Materials Transactions A, 2009, 40(1): 24-35. [4]Babu S S, Miller M K, Vitek J M, et al. Characterization of the microstructure evolution in a nickel base superalloy during continuous cooling conditions[J]. Acta Materialia, 2001, 49(20): 4149-4160. [5]Sarosi P M, Wang B, Simmons J P, et al. Formation of multimodal size distributions of γ′ in a nickel-base superalloy during interrupted continuous cooling[J]. Scripta Materialia, 2007, 57(8): 767-770. [6]Wen Y H, Simmons J P, Shen C, et al. Phase-field modeling of bimodal particle size distributions during continuous cooling[J]. Acta Materialia, 2003, 51(4): 1123-1132. [7]Wen Y H, Wang B, Simmons J P, et al. A phase-field model for heat treatment applications in Ni-based alloys[J]. Acta Materialia, 2006, 54(8): 2087-2099. [8]Singh A R P, Nag S, Chattopadhyay S, et al. Mechanisms related to different generations of γ′ precipitation during continuous cooling of a nickel base superalloy[J]. Acta Materialia, 2013, 61(1): 280-293. [9]Singh A R P, Nag S, Hwang J Y, et al. Influence of cooling rate on the development of multiple generations of γ′ precipitates in a commercial nickel base superalloy[J]. Materials Characterization, 2011, 62(9): 878-886. [10]Radis R, Schaffer M, Albu M, et al. Multimodal size distributions of γ′ precipitates during continuous cooling of UDIMET 720 Li[J]. Acta Materialia, 2009, 57(19): 5739-5747. [11]Sarosi P M, Wang B, Simmons J P, et al. Formation of multimodal size distributions of γ′ in a nickel-base superalloy during interrupted continuous cooling[J]. Scripta Materialia, 2007, 57(8): 767-770. [12]Mitchell R J, Preuss M, Hardy M C, et al. Influence of composition and cooling rate on constrained and unconstrained lattice parameters in advanced polycrystalline nickel—base superalloys[J]. Materials Science and Engineering A, 2006, 423(1/2): 282-291. [13]Zhao S, Xie X, Smith G D, et al. Microstructural stability and mechanical properties of a new nickel-based superalloy[J]. Materials Science and Engineering A, 2003, 355(1/2): 96-105. [14]Zhao S, Xie X, Smith G D, et al. Research and improvement on structure stability and corrosion resistance of nickel-base superalloy INCONEL alloy 740[J]. Materials and Design, 2006, 27(10): 1120-1127. [15]李振江, 肖纳敏, 李殿中, 等. G18CrMo2-6钢回火组织及冲击韧性研究[J]. 金属学报, 2014, 50(7): 777-786. Li Zhenjiang, Xiao Namin, Li Dianzhong, et al. Influence of microstructure on impact toughness of G18CrMo2-6 steel during tempering[J]. Acta Metallurgical Sinica, 2014, 50(7): 777-786. [16]Ricker R E, Hall D E, Fink J L. The effect of aqueous environments on the fracture behavior of ductile nickel aluminide[J]. Scripta Metallurgica et Materialia, 1990, 24(2): 291-296. [17]Grove C A, Petzold L D. Mechanisms of stress-corrosion cracking of alloy X-750 in high-purity water[J]. Journal of Materials for Energy Systems, 1985, 7(2): 147-162. [18]Valle J A D, Picasso A C, Alvarez I, et al. Age-hardening behavior of Inconel X-750 superalloy[J]. Scripta Materialia, 1999, 41(3): 237-243. [19]Valle J A D, Romero R, Picasso A C. Bauschinger effect in age-hardened Inconel X-750 alloy[J]. Materials Science and Engineering A, 2001, 311(1/2): 100-107. [20]赵双群, 董建新, 谢锡善. Ni-Cr-Co基高温合金704 ℃和760 ℃时效组织稳定性[J]. 中国有色金属学报, 2003(3): 565-569. Zhao Shuangqun, Dong Jianxin, Xie Xishan. Structure stability of Ni-Cr-Co base superalloy aged at 704 ℃ and 760 ℃[J]. The Chinese Journal of Nonferrous Metals, 2003(3): 565-569. [21]侯介山, 郭建亭, 周兰章, 等. K44镍基高温合金长期时效过程中γ′相粗化对拉伸性能的影响[J]. 金属学报, 2006(5): 481-486. Hou Jieshan, Guo Jianting, Zhou Lanzhang, et al. Effects of γ'-precipitate coarsening on tensile properties of Ni base superalloy K44 during long-term aging[J]. Acta Metallurgica Sinica, 2006(5): 481-486. |