[1] 张 栋,钟培道,陶春虎,等.效分析[M].北京:国防工业出版社,2009:202. Zhang Dong,Zhong Peidao,Tao Chunhu,et al.Failure Analysis[M].Beijing:National Defense Industry Press,2009:202. [2] 刘昌奎,臧金鑫,张 兵.30CrMnSiA螺栓断裂原因分析[J].失效分析与预防,2008,3(2):42-47. Liu Changkui,Zang Jinxin,Zhang Bing.Failure analysis of 30CrMnSiA bolt fracture[J].Failure Analysis and Prevention,2008,3(2):42-47. [3] 李家鼎,吴素君,史青君,等.双动滑阀螺栓断裂失效分析[J].失效分析与预防,2006,1(4):43-45. Li Jiading,Wu Sujun,Shi Qingjun,et al.Failure analysis of bolt in two way moving slide valve[J].Failure Analysis and Prevention,2006,1(4):43-45. [4] 燕 翔,李 娜.自制螺栓表面裂纹成因分析[J].失效分析与预防,2010,5(4):243-246. Yan Xiang,Li Na.Analysis on surface cracks of self-made bolt[J].Failure Analysis and Prevention,2010,5(4):243-246. [5] 胡春燕,刘星灵,陈 星.高强度钢螺栓断裂失效分析[J].金属热处理,2012,37(9):126-127. Hu Chunyan,Liu Xingling,Chen Xing.Failure analysis of high strength steel bolts fracture[J].Heat Treatment of Metals,2012,37(9):126-127. [6] 李平平.轮毂螺栓断裂分析及预防措施[J].金属热处理,2019,44(S1):127-151. Li Pingping.Fracture analysis and preventive measures of hub bolts[J].Heat Treatment of Metals,2019,44(S1):127-151. [7] 龙必查.8.8级汽配螺杆氢脆的技术分析[J].热处理技术与装备,2017,38(6):16-18. Long Bicha.Technical analysis of hydrogen embrittlement in 8.8 grade auto accessory screw[J].Heat Treatment Technology and Equipment,2017,38(6):16-18. [8] 吴建国.氢气对金属材料之影响[J].材料导报,2004(18):119-120. Wu Jianguo.Hydrogen effect on metal materials[J].Materials Reports,2004(18):119-120. [9] Ham J O,Jang Y H,Lee G P,et al.Evaluation method of sensitivity of hydrogen embrittlement for high strength bolts[J].Materials Science and Engineering A,2013,581:83-89. [10] 穆妍君,杨 峻,文翰剡.30CrMnSiA钢螺栓的断裂失效分析[J].金属热处理,2014,39(1):141-143. Mu Yanjun,Yang Jun,Wen Hanyan.Fracture failure analysis of 30CrMnSiA steel bolts[J].Heat Treatment of Metals,2014,39(1):141-143. |