[1] 戴真全. 347H奥氏体不锈钢的焊接热裂纹和再热裂纹[J]. 化工设备与管道, 2010, 47(3): 54-58. Dai Zhenquan. Heat crack and reheat crack in weld in austenitic steel 347H[J]. Process Equipment and Piping, 2010, 47(3): 54-58. [2] 谷 宇, 孙铭山, 范光伟. 铌含量对17%Cr超纯铁素体不锈钢组织与高温强度的影响[J]. 钢铁, 2011, 46(1): 71-74, 85. Gu Yu, Sun Mingshan, Fan Guangwei. Effect of Nb content on microstructure and high temperature strength of 17%Cr ferritic stainless steel[J]. Iron and Steel, 2011, 46(1): 71-74, 85. [3] 张朝晖, 柳永宁, 金 波, 等. 铌微合金钢形变连续冷却过程中的相变[J]. 机械工程材料, 2007, 31(4): 85-88. Zhang Zhaohui, Liu Yongning, Jin Bo, et al. Continuous cooling transformation of Nb micro-alloyed steel after deformation[J]. Materials for Mechanical Engineering, 2007, 31(4): 85-88. [4] 王新华, 昌 波, 李景捷, 等. 700-1000 ℃间含Nb钢铸坯的延塑性降低与Nb(C, N)析出[J]. 金属学报, 1997, 33(5): 485-491. Wang Xinhua, Chang Bo, Li Jingjie, et al. Ductility loss and Nb(C,N) precipitation in Nb-containing steel slab in the temperature range from 700 to 1000 ℃[J]. Acta Metallrugica Sinica, 1997, 33(5): 485-491. [5] 李新梅, 张忠文, 杜宝帅, 等. 长期高温服役后S31042奥氏体耐热钢的微观组织[J]. 金属热处理, 2019, 44(4): 171-174. Li Xinmei, Zhang Zhongwen, Du Baoshuai, et al. Microstructure of S31042 austenite heat resistant steel after long-term service under high temperature[J]. Heat Treatment of Metals, 2019, 44(4): 171-174. [6] Lseda A, Okada H, Semba H, et al. Long term creep properties and microstructure of SUPER304H, TP347HFG and HR3C for A-USC boilers[J]. Energy Materials, 2007, 2(4): 199-206. [7] Viswanathan R, Coleman K, Rao U. Materials for ultra-supercritical coal-fired power plant boilers[J]. International Journal of Pressure Vessels and Piping, 2006, 83(11): 778-783. [8] 杜宝帅, 刘 睿, 张忠文, 等. 高温长时服役HR3C钢焊接接头的组织与性能[J]. 金属热处理, 2015, 40(2): 52-55. Du Baoshuai, Liu Rui, Zhang Zhongwen, et al. Microstructure and properties of HR3C steel weld joint exposed to elevated temperature for long-term[J]. Heat Treatment of Metals, 2015, 40(2): 52-55. [9] 张文华. 不锈钢及其热处理[M]. 沈阳: 辽宁科学技术出版社, 2010. [10] 杜 伟, 孙全社, 江来珠, 等. 铌与钛对铁素体不锈钢析出和成形性的影响[J]. 钢铁研究学报, 2010, 22(3): 48-51. Du Wei, Sun Quanshe, Jiang Laizhu, et al. Effect of Nb and Ti on precipitation and formability of ferritic stainless steel[J]. Journal of Iron and Steel Research, 2010, 22(3): 48-51. [11] 康永海, 李具仓. 304L和321不锈钢耐腐蚀性能研究[J]. 热加工工艺, 2015, 44(6): 81-88. Kang Yonghai, Li Jucang. Corrosion resistance of 304L and 321 stainless steel[J]. Hot Working Technology, 2015, 44(6): 81-88. [12] 张泽磊, 姚正军, 张平则, 等. 冷弯加工对国产301L不锈钢耐点蚀性能的影响[J]. 中国冶金, 2015, 25(7): 5-9. Zhang Zelei, Yao Zhengjun, Zhang Pingze, et al. Influence of cold bending process on pitting corrosion resistance of domestic 301L stainless steel[J]. China Metallurgy, 2015, 25(7): 5-9. [13] 孙 涛, 邓 博, 徐菊良, 等. 氮、铌添加对奥氏体不锈钢电化学腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2010, 30(6): 421-425. Sun Tao, Deng Bo, Xu Juliang, et al. Influence of niobium and nitrogen on the resistance to pitting and intergranular corrosion of 304 austenitic stainless steel[J]. Journal of Chinese Society for Corrosion and Protection, 2010, 30(6): 421-425. [14] 宁小智, 邢长军, 雍歧龙, 等. 氮含量对无镍奥氏体不锈钢理化性能的影响[J]. 中国冶金, 2019, 29(6): 34-37. Ning Xiaozhi, Xing Changjun, Yong Qilong, et al. Effects of nitrogen content on physical and chemical properties of nickel-free austenitic stainless steels[J]. China Metallurgy, 2019, 29(6): 34-37. |