合金元素对高碳珠光体盘条钢组织和性能的影响

唐恩1, 彭侠超2, 刘红亮3, 张瑞1, 王坤1   

  1. 1.浙江工贸职业技术学院, 浙江 温州 325000;
    2.兰州理工大学 材料科学与工程学院, 甘肃 兰州 730000;
    3.大自然钢业集团有限公司, 浙江 温州 325000
  • 收稿日期:2023-10-24 修回日期:2024-02-28 出版日期:2024-04-25 发布日期:2024-05-27
  • 通讯作者: 张 瑞,副教授,硕士,E-mail:76191033@qq.com
  • 作者简介:唐 恩(1979—),男,教授,博士,主要研究方向为金属材料加工,E-mail:tangen@zjitc.edu.cn。
  • 基金资助:
    浙江工贸引进人才项目(YJRC202206)

Effect of alloying elements on microstructure and properties of high carbon pearlite wire rod steel

Tang En1, Peng Xiachao2, Liu Hongliang3, Zhang Rui1, Wang Kun1   

  1. 1. Zhejiang Industry & Trade Vocational College, Wenzhou Zhejiang 325000, China;
    2. School of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou Gansu 730000, China;
    3. Natural Steel Group Co., Ltd., Wenzhou Zhejiang 325000, China
  • Received:2023-10-24 Revised:2024-02-28 Online:2024-04-25 Published:2024-05-27

摘要: 设计了3种不同微合金元素V、Nb含量的高碳钢盘条钢,通过拉伸性能测试、组织观察、母相奥氏体晶粒尺寸统计等分析了微合金元素对盘条钢的强化作用。结果表明,V钢的抗拉强度为1282.7 MPa,总延伸率为13.08%,相比于基础钢强度增加约156.5 MPa,总延伸率略有提高。V+高Nb钢的抗拉强度为1287.0 MPa,总延伸率为12.38%,相比于基础钢强度增加约160.8 MPa,总延伸率提高0.25%。对于高碳珠光体钢,添加适量V可以起到细化珠光体片层间距的作用,但是继续添加Nb并不会进一步细化珠光体片层间距,对于抗拉强度的提升无显著作用,因此加入0.1%V后无需再加Nb。微合金元素V的添加除了细化母相奥氏体晶粒,还提升了盘条钢的加工硬化能力,主要是由于珠光体片层间距得到细化,终端盘条钢成品表现出较好抗变形能力。

关键词: 微合金元素, 珠光体, 片层间距, 拉伸性能, 母相奥氏体

Abstract: Three kinds of high carbon wire rod steels with different content of microalloying elements V, Nb were designed. The strengthening effects of microalloying elements on the wire rod steel were analyzed through tensile testing, microstructure observation and prior austenite grain size statistics. The results show that the tensile strength of the V-steel is 1282.7 MPa, which is increased by 156.5 MPa compared with the base steel and accompanied with a slight increase of total elongation of 13.08%. The tensile strength and total elongation of the V+high Nb steel are 1287.0 MPa and 12.38%, which are increased by 160.8 MPa and 0.25% compared with the base steel, respectively. For high-carbon pearlitic steel, adding an appropriate amount of V can refine the pearlite lamellar spacing, however, adding more Nb will not further refine the pearlite lamellar spacing. Besides, the more addition of Nb has no significant effect on the improvement of tensile strength. Therefore, there is no need to add Nb after adding 0.1%V in the high carbon pearlite wire rod. The addition of microalloying element V not only refines the prior austenite grain, but also improves the work-hardening ability of the wire rod steel, mainly because the pearlite lamellar spacing is refined, so that it shows better deformation resistance.

Key words: microalloy, pearlite, lamellar spacing, tensile property, parent austenite