[1]肖 寒, 于佳新, 张宏宇, 等. 退火温度对新型高强耐蚀钛合金组织与性能的影响[J]. 稀有金属材料与工程, 2022, 51(3): 947-952. Xiao Han, Yu Jiaxin, Zhang Hongyu, et al. Effects of annealing temperature on microstructure and properties of new high strength corrosion resistant titanium alloy[J]. Rare Metal Materials and Engineering, 2022, 51(3): 947-952. [2]李志尚, 陈立全, 杨 平, 等. TC18钛合金棒材锻造时拔长过程织构模拟[J]. 塑性工程学报, 2021, 28(9): 94-102. Li Zhishang, Chen Liquan, Yang Ping, et al. Simulation of texture in drawing of TC18 titanium alloy bars during forging[J]. Journal of Plasticity Engineering, 2021, 28(9): 94-102. [3]Cui Yimin, Zheng Weiwei, Hua Chao, et al. Effectiveness of hot deformation and subsequent annealing for β grain refinement of Ti-5Al-5Mo-5V-1Cr-1Fe titanium alloy[J]. Rare Metals, 2021, 40(12): 3608-3615. [4]牟芃威, 吕书锋, 杜赵新. 固溶和时效温度对铸态TC18合金组织性能的影响[J]. 钢铁钒钛, 2023, 44(2): 61-66. Mou Pengwei, Lü Shufeng, Du Zhaoxin. Effects of solution and aging temperature on microstructure and properties of as-cast TC18 alloy[J]. Iron Steel Vanadium Titanium, 2023, 44(2): 61-66. [5]辛宏靖, 廖敏茜, 王潇汉, 等. 初生α相含量对TC18时效组织及力学性能的影响[J]. 精密成形工程, 2021, 13(3): 143-147. Xin Hongjing, Liao Minxi, Wang Xiaohan, et al. Effect of volume fraction of primary α phase on mechanical property in TC18 alloy[J]. Journal of Netshape Forming Engineering, 2021, 13(3): 143-147. [6]张 颖, 胡生双, 郑 超, 等. 双重退火对激光增材制造TC18钛合金组织和性能的影响[J]. 特种铸造及有色合金, 2021, 41(8): 1006-1009. Zhang Ying, Hu Shengshuang, Zheng Chao, et al. Effects of double annealing on microstructure and properties of TC18 titanium alloy by laser additive manufacturing[J]. Special Casting and Nonferrous Alloys, 2021, 41(8): 1006-1009. [7]张 翥, 王群骄, 莫 畏. 钛的金属学和热处理[M]. 北京: 冶金工业出版社, 2009: 46-220. [8]辛社伟, 赵永庆. 钛合金固态相变的归纳与讨论(Ⅵ)—阿尔法[J]. 钛工业进展, 2013, 30(4): 1-8. Xin Shewei, Zhao Yongqing. Inductions and discussions of solid state phase transformation of titanium alloy(Ⅵ)-Alpha[J]. Titanium Industry Progress, 2013, 30(4): 1-8. [9]辛社伟. 钛合金固态相变的归纳与讨论(Ⅴ)—相与相变谈[J]. 钛工业进展, 2013, 30(3): 12-15. Xin Shewei. Inductions and discussions of solid state phase transformation of titanium alloy(Ⅴ)-Talking about phase and phase-transformation[J]. Titanium Industry Progress, 2013, 30(3): 12-15. [10]王 琛, 徐 栋, 陈 力. 热处理对TC18钛合金组织和力学性能的影响[J]. 金属热处理, 2018, 43(9): 186-190. Wang Chen, Xu Dong, Chen Li. Effect of heat treatment on microstructure and mechanical properties of TC18 titanium alloy[J]. Heat Treatment of Metals, 2018, 43(9): 186-190. [11]Xu Jianwei, Zeng Weidong, Zhou Dadi, et al. Evolution of coordination between α and β phases for two-phase titanium alloy during hot working[J]. Transactions of Nonferrous Metals Society of China, 2021, 31(11): 3428-3438. [12]李少强, 陈 威, 查 友, 等. TC18合金大型锻棒冲击韧性的横纵向差异研究[J]. 稀有金属材料与工程, 2021, 50(3): 911-917. Li Shaoqiang, Chen Wei, Zha You, et al. Difference between transverse and longitudinal impact toughness of TC18 alloy large-scale forging rods[J]. Rare Metal Materials and Engineering, 2021, 50(3): 911-917. [13]Chi G, Yi D, Jiang B, et al. Crack propagation during Charpy impact toughness testing of Ti-AlV-Mo-Zr alloy tubes containing equiaxed and lamellar microstructures[J]. Journal of Alloys and Compounds, 2020, 852: 156581. [14]Wang X, Zhu Z, Lu T, et al. The Influence of forging processing on fatigue crack propagation rate of damage-tolerant titanium alloy[J]. Rare Metals Letters, 2008, 27(7): 12-20. [15]Guo P, Zhao Y, Hong Q, et al. Fatigue crack propagation and crack tip plasticity zone of TC4-DT titanium alloy[J]. Rare Metal Materials and Engineering, 2014, 43(6): 1479-1482. [16]Nitin Kotkunde, Hansoge Nitin Krishnamurthy, Pavan Puranik, et al. Microstructure study and constitutive modeling of Ti-6Al-4V alloy at elevated temperatures[J]. Materials & Design, 2014, 54: 96-103. [17]刘莹莹, 张君彦, 王梦婷, 等. TC18钛合金棒材和锻件的冲击性能及断口分析[J]. 稀有金属, 2019, 43(8): 891-896. Liu Yingying, Zhang Junyan, Wang Mengting, et al. Impact properties and fracture analysis of TC18 titanium alloy bars and forgings[J]. Chinese Journal of Rare Metals, 2019, 43(8): 891-896. [18]Liu Z, Li P, Xiong L, et al. High-temperature tensile deformation behavior and microstructure evolution of Ti55 titanium alloy[J]. Materials Science and Engineering A, 2016, 680: 259-269. [19]Chen Junhong, Xu Weifang, Zhang Fangju, et al. Strain rate dependent tension behavior of TC11 titanium alloys[J]. Rare Metal Materials and Engineering, 2021, 50(6): 1883-1889. [20]Wang He, Ma Shuyuan, Wang Jiachen, et al. Microstructure and mechanical properties of TA15/TC11 graded structural material by wire arc additive manufacturing process[J]. Transactions of Nonferrous Metals Society of China, 2021, 31(8): 2323-2335. |