中间退火温度对Fe-3wt%Si取向硅钢抑制剂演变的影响
鞠芳1,2,金自力1,任慧平1,宋正会2,白海瑞1,侯景利1
Effect of intermediate annealing temperature on inhibitors of Fe-3wt%Si grain-oriented silicon steel
Ju Fang1, 2, Jin Zili1, Ren Huiping1, Song Zhenghui1, Bai Hairui1, Hou Jingli1
金属热处理 . 2015, (3): 82 -85 .  DOI: 10.13251/j.issn.0254-6051.2015.03.019