[1] |
Su Yong, Wang Shuai, Wang Jixing, Yu Xingfu, Liu Hongxiu, Liu Jinling.
Effect of compound chemical heat treatment on microstructure and hardness of G13Cr4Mo4Ni4V steel
[J]. Heat Treatment of Metals, 2022, 47(4): 226-230.
|
[2] |
Yang Jie, Wang Xi, Zhou Jie, Wu Jianxiang, Qu Zhiyuan, Dai Heping, Peng Haijun.
Formation mechanism of quenching cracks in branch-shaped structure of steering knuckle forgings
[J]. Heat Treatment of Metals, 2022, 47(4): 263-267.
|
[3] |
Dong Rui, Chen Lin, Cen Yaodong, Bao Xirong.
Microstructure and fatigue crack growth of a bainitic steel under different heat treatments
[J]. Heat Treatment of Metals, 2022, 47(2): 153-158.
|
[4] |
Lü Jinyi, Zhang Yiwei, Luo Xiaobing, Yuan Xiaomin.
In-situ observation of austenite continuous cooling transformation characteristics of Cu-bearing steel
[J]. Heat Treatment of Metals, 2022, 47(1): 19-24.
|
[5] |
Wang Chunhua,Wang Feng , Wang Fengliang, Fang Hongjie, Yang Lijuan.
Effect of multi-stage solid solution treatment on microstructure and properties of 7136-0.35La aluminum alloy
[J]. Heat Treatment of Metals, 2021, 46(9): 124-128.
|
[6] |
Zhou Jianbo, Zhang Jing, Zhang Leitao, Li Haitao, Fan Shuaiqi, Xu Jinfu.
Effect of laser process parameters on crack rate and microstructure of Ni60/WC clad coating
[J]. Heat Treatment of Metals, 2021, 46(9): 252-257.
|
[7] |
Shi Keqing, Guo Fu, An Longsen, Chen Yun, Du Ziyang, Wu Meng, Xu Qinpei.
Heat treatment process of 42CrMo4 steel wind power main shaft
[J]. Heat Treatment of Metals, 2021, 46(8): 201-204.
|
[8] |
Nie Xiaolong, Gao Jiaqiang, Meng Kairen, Wang Junyi, Liu Xinkuan.
Fracture failure analysis of 60Si2Mn spring steel
[J]. Heat Treatment of Metals, 2021, 46(8): 246-249.
|
[9] |
Xu Hongxiang, Wang Hongwei, Zhang Heng, Wang Jun, Zhao Shaofu.
Crack analysis of case-hardened 20Cr2Ni4 steel gear after assembly
[J]. Heat Treatment of Metals, 2021, 46(8): 250-253.
|
[10] |
Yang Qingxu, Wang Xue, Ma Junpeng, Yang Chao.
Crack analysis of T23/12Cr1MoV dissimilar steel welded joints during PWHT in the water-wall of USC boiler
[J]. Heat Treatment of Metals, 2021, 46(7): 218-222.
|
[11] |
Song Quan, Dan Ting, Li Xiaoguang, Gao Mingsen, Cao Huihui.
Fracture cause analysis of W6Mo5Cr4V2Al high speed steel twist drill
[J]. Heat Treatment of Metals, 2021, 46(7): 229-232.
|
[12] |
Lü Jing, Yang Qiquan, Zhang Qian, Hu Jie, Xu Xin.
Cause analysis of cracks in bolt holes of cast steel wheel-mounted brake disc
[J]. Heat Treatment of Metals, 2021, 46(7): 238-241.
|
[13] |
Ji Guoqiang, Ge Guiming, Yu Lijuan, Zhong Jizhi.
Analysis on cracking of 50CrV4 steel washer
[J]. Heat Treatment of Metals, 2021, 46(7): 254-257.
|
[14] |
Wang Lingqi, He Yanlin, Pan Le.
Effect of tempering temperature on microstructure and mechanical properties of high nitrogen stainless bearing steel
[J]. Heat Treatment of Metals, 2021, 46(6): 8-13.
|
[15] |
Li Xiong, Lin Faju, Du Simin, Wu Chengchuan.
Comparative analysis of high performance bearing steels
[J]. Heat Treatment of Metals, 2021, 46(6): 14-20.
|