[1] |
Zhao Ping.
Cause analysis for cracking of high temperature superheater tubes in supercritical circulating fluidized bed boiler
[J]. Heat Treatment of Metals, 2021, 46(6): 225-230.
|
[2] |
Meng Dianwu, Zhang Jiantang, Shen Nan, Hu Xuefei, Lu Yu, Du Xiaodong.
New supersonic arc spraying coating for boiler water wall protection
[J]. Heat Treatment of Metals, 2020, 45(4): 183-187.
|
[3] |
Zhou Renyuan, Zhu Lihui, Li Shixian, Zhai Guoli, Song Ming.
Reheat cracking susceptibility of modified T23 steel
[J]. HTM, 2020, 45(1): 20-25.
|
[4] |
Xu Kai1, He Cheng2, Li Wensheng2, Zhao Jianping2, Ai Hong2, Zhang Siwen2, Shi Baoliang3, Ren Ai3.
Aging law of T23 steel final superheater tube serviced for different time
[J]. HTM, 2016, 41(8): 45-51.
|
[5] |
Wang Wei1, Wang Zhiwu2, Li Wensheng1, Tian Jing2, Zhong Wanli1, Song Tao2, Lin Jiedong1.
Thermodynamic equilibrium phases of TP347H steel with different contents of Cr and Ni
[J]. HTM, 2016, 41(10): 99-101.
|
[6] |
Li Zhenliang, Wang Jia’an, Xiao Minyan.
Failure analysis of SA-213TP347H steel reheater tube
[J]. HTM, 2015, 40(8): 191-194.
|
[7] |
Yuan Xiaomin, Hu Shanshan, Zhang Yiwei, Yang Lei.
Effects of controlled cooling process on microstructure and mechanical properties of 12Cr1MoV boiler steel
[J]. HTM, 2015, 40(6): 116-120.
|
[8] |
Qing Hui, Ren Yaojian, Sun Zhi.
Burst failure analysis on 20G low temperature superheater tube of biomass-fired boiler
[J]. HTM, 2014, 39(9): 144-147.
|
[9] |
Zhang Yiwei, Yuan Xiaomin, Zheng Zhen.
Effect of controlled cooling process on microstructure of 20G boiler steel
[J]. HTM, 2014, 39(2): 93-96.
|