[1] |
Yang Jie, Wang Xi, Zhou Jie, Wu Jianxiang, Qu Zhiyuan, Dai Heping, Peng Haijun.
Formation mechanism of quenching cracks in branch-shaped structure of steering knuckle forgings
[J]. Heat Treatment of Metals, 2022, 47(4): 263-267.
|
[2] |
Shi Keqing, Guo Fu, An Longsen, Chen Yun, Du Ziyang, Wu Meng, Xu Qinpei.
Heat treatment process of 42CrMo4 steel wind power main shaft
[J]. Heat Treatment of Metals, 2021, 46(8): 201-204.
|
[3] |
Jiao Li, Shang Haikun, He Jianfeng, Zhao Yingjun, Zhang Weimin, Li Weimin, Zhou Lanmei.
Fracture failure analysis of 42CrMo steel high strength bolts for diesel engine
[J]. Heat Treatment of Metals, 2021, 46(6): 245-249.
|
[4] |
Mi Pei, Sun Yongpeng, Zhang Yong.
Causes and improvement methods of induction quenching cracks in mining toothed rail
[J]. Heat Treatment of Metals, 2021, 46(6): 250-252.
|
[5] |
Zhang Jiawen, Fu Tianliang, Wu Hao, Wang Zhaodong.
Cause analysis on quenching cracking of 40CrNiMo7 steel forged shaft
[J]. Heat Treatment of Metals, 2021, 46(2): 213-217.
|
[6] |
Cheng Yuan, Hu Fangzhong, Yang Shaopeng, Wang Kaizhong, Jin Guozhong, Chen Shijie, Wang Lianglin.
Cracking failure analysis of 40Cr steel forgings for automobile front axle
[J]. Heat Treatment of Metals, 2021, 46(12): 294-297.
|
[7] |
Yuan Jingzhi, Shi Yuezhi, Xu Wenhua, Chen Lubin, Lü Yupeng.
Structure-defect analysis of crack failure in 42CrMo wind power spindle
[J]. Heat Treatment of Metals, 2020, 45(7): 206-209.
|
[8] |
Yang Hongquan, Xu Xiangjiu, Zhou Jingcao.
Analysis on quenching cracks of SA-387Gr.91 steel spherical head
[J]. Heat Treatment of Metals, 2020, 45(7): 219-223.
|
[9] |
Dong Dengchao, Zhang Ke, Wu Yuanyuan, Hong Huimin.
Cracking analysis of wearable steel ball during ball falling test
[J]. HTM, 2017, 42(4): 200-203.
|
[10] |
Wang Changjian.
Failure analysis of quenching cracks of 45 steel taper sleeve
[J]. HTM, 2017, 42(4): 204-207.
|
[11] |
Jiao Donfeng1, Jin Linkui2.
Cause analysis on median frequency quenching cracking and melting of 40Cr steel semi axle
[J]. HTM, 2016, 41(3): 210-213.
|
[12] |
Jiang Rusong1, Liao Yonghong2.
Quenching crack analysis and counter measures of 40CrMnMo steel single pump body
[J]. HTM, 2016, 41(12): 187-191.
|
[13] |
Zhang Liwei, Liu Sufen, Wang Fan, Ren Xiangyu, Zhang Zhiwei, Wen Tieli, Zhao Yudong.
Analysis on quenching cracks of 50CrVA steel leaf spring
[J]. HTM, 2015, 40(12): 201-203.
|
[14] |
Wang Changjian.
Cause analysis and counter measure of fracturing pump head crack
[J]. HTM, 2014, 39(9): 151-154.
|
[15] |
Qi Guoquan, Li Xunji, Qiang Yuan, Wang Fushan.
Failure analysis of P110 casing crack in hydrostatic proof test
[J]. HTM, 2014, 39(7): 166-169.
|