Heat Treatment of Metals ›› 2024, Vol. 49 ›› Issue (9): 96-102.DOI: 10.13251/j.issn.0254-6051.2024.09.016

• PROCESS RESEARCH • Previous Articles     Next Articles

Evolution of LPSO phase and properties of Mg-Y-Gd-Zn-Zr alloy at different aging temperatures

Ren Guangxiao1, Wang Chao2,3, Cao Xijuan1, Wang Kai2, Wang Hongxia1,2, Cheng Weili2, Niu Xiaofeng2   

  1. 1. Shanxi Province Pilot Base for Research and Development of Light Metals and Their Composite Materials and Structured Applications, Shanxi Jianghuai Heavy Industry Co., Ltd., Jincheng Shanxi 048000, China;
    2. Shanxi Key Laboratory of Advanced Magnesium-Based Materials, College of Materials Science and Engineering, Taiyuan University of Technology, Taiyuan Shanxi 030024, China;
    3. Avic Shaanxi Hongyuan Aviation Forging Company Ltd., Xi'an Shaanxi 710000, China
  • Received:2024-05-12 Revised:2024-08-09 Online:2024-09-25 Published:2024-10-29

Abstract: The microstructural evolution of the Mg-6Y-3Gd-3Zn-0.5Zr alloys in the as-cast, solid solution and aging states and its influence on the mechanical properties were investigated by using OM, SEM, XRD, TEM and property testing methods. The results show that the as-cast alloy consists of dendritic α-Mg matrix with a continuous network of 18R-LPSO and Mg24(Gd, Y, Zn)5 mixed phases at the grain boundaries. After solid solution treatment, the most of Mg24(Gd, Y, Zn)5 phase and part of the 18R-LPSO phase are dissolved back into the matrix. A large amount of lamellar 14H-LPSO and Mg3(Y, Gd) and Mg5(Y, Gd) phases are precipitated in the matrix after aging at 250 ℃ and 300 ℃. Only 14H-LPSO phase is precipitated in the crystals after aging at 400 ℃. The tensile strength and elongation of the as-cast alloy are 222.7 MPa and 4.1%, respectively. The strength of the alloy decreases and the elongation increases slightly after aging. The alloy peak aged at 400 ℃ shows the greatest decrease in strength due to the large number and size of 14H-LPSO precipitated in the crystals, and the tensile strength decreases by 39 MPa compared with that of the as-cast state.

Key words: Mg-Y-Gd-Zn-Zr alloy, LPSO phase, heat treatment, mechanical properties