[1] |
Sun Guojin, Gao Zhiwen, Cui Xiaoyan, Gao Kekun, Sun Li.
Effect of dual liquid quenching on microstructure and hardness of 9Cr2Mo steel roller
[J]. Heat Treatment of Metals, 2022, 47(3): 88-91.
|
[2] |
Zhao Yantao, Jiang Zeyi, Zhang Xinru, Wang Dijie.
Temperature uniformity of aluminum plate during double-sided jet heating and roller swing
[J]. Heat Treatment of Metals, 2022, 47(1): 178-184.
|
[3] |
Hu Wenxiang, Li Jianxin, Shi Zhengliang, Xu Jia, Guan Yunqi, Ding Shaopeng.
Effect of cryogenic treatment on microstructure and wear resistance of alloy cast iron
[J]. Heat Treatment of Metals, 2021, 46(7): 168-172.
|
[4] |
Zhao Haiqiang, Chen Hongye.
Formation mechanism and preventive measures of pitting defects on surface of cold rolled continuous annealing strip steel
[J]. Heat Treatment of Metals, 2020, 45(6): 236-238.
|
[5] |
Liu Xiaodong, Jiang Honglei, Xie Meng.
Analysis on residual stress of Q345 steel in laser cladding process
[J]. HTM, 2020, 45(3): 226-230.
|
[6] |
Cao Yu, Song Xinli, Zhen Aiqin, Chen Rongdong, Jia Juan, Bi Yunjie.
Effect of heat treatment process on microstructure and hardness of high chromium cast iron roller produced by centrifuge casting
[J]. HTM, 2020, 45(2): 108-113.
|
[7] |
Li Tingting1, Zhou Yueming2, Shu Da1.
Simulation of induction heating and temperature distribution on roller surface during warm rolling
[J]. HTM, 2016, 41(8): 165-169.
|
[8] |
Li Pingping,Chen Kaimin,Wu Jianhua,Xu Luoping, Liang huilei.
Surface defects analysis of guide roller and counter measures
[J]. HTM, 2016, 41(6): 185-187.
|
[9] |
Guo Wei1,2,Chu Zuoming1,Jin Kang1,Wang Xiaohui1,Chen Dong1,Zhou Yingli1.
Process parameter control?of water quenching and oil cooling for MC3 steel cold work roller
[J]. HTM, 2016, 41(5): 137-141.
|
[10] |
Zhang Jingkui, Dong Hua, Zhou Enze.
Optimization of water flow and roller velocity at high-pressure water injection zone of roller-type quenching machine
[J]. HTM, 2016, 41(12): 164-167.
|
[11] |
Liang Zhiqiang1,Zhang Ling1,2, WangYujie1, Zeng Chaofan1,2, Sun Wei1,2.
Analysis of material and heat treatment quality for roller of foreign mill bearing
[J]. HTM, 2016, 41(10): 202-205.
|
[12] |
Xu Shujiao1,Xu Xinhua1,Chen Guoxi 1,Qin Wei 1,ShengJiansheng1,Cheng Yang1,Deng Qilin2.
Fracture failure analysis of 21CrMoV5.11 steel continuous casting roller
[J]. HTM, 2016, 41(1): 232-235.
|
[13] |
He Wei1, Hao Guanghui1, Wei Qinwen2, Hu Yumao1, Chen Yang1, He Junchao1.
Numerical simulation of laser hardening of 42CrMo steel spherical fixed set bearing in roller bit
[J]. HTM, 2015, 40(8): 149-153.
|
[14] |
Xu Jingtian, Cheng Ruizhou, Zhao Xiaojiao.
Control system design of vacuum annealing furnace based on S7-300 PLC
[J]. HTM, 2015, 40(8): 199-203.
|
[15] |
Wang Jiangang1, Hu Jianwen1, Mao Lei1,2, Qin Sen1, Wang Jintong3.
Surface strengthening of corrugated roller
[J]. HTM, 2015, 40(7): 148-152.
|