[1]李秀景, 王淑华, 张 星, 等. 薄板坯热连轧工艺对65Mn钢带组织和性能的影响[J]. 钢铁钒钛, 2020, 41(6): 158-163. Li Xiujing, Wang Shuhua, Zhang Xing, et al. Effect of FTSR hot rolling process on microstructure and mechanical properties of 65Mn strip[J]. Iron Steel Vanadium Titanium, 2020, 41(6): 158-163. [2]李广林, 陈凌峰, 胡志远, 等. 原料边部组织和力学性能对冷轧的影响分析[J]. 中国冶金, 2015, 25(3): 33-36. Li Guanglin, Chen Lingfeng, Hu Zhiyuan, et al. Effects analysis of the edge tissue and mechanical capability of raw material to the cold-rolling[J]. China Metallurgy, 2015, 25(3): 33-36. [3]曹晓恩, 赵红旗, 李守华, 等. 980 MPa级冷轧超高强度双相钢边裂原因分析与工艺优化[J]. 中国冶金, 2022, 32(9): 90-96. Cao Xiaoen, Zhao Hongqi, Li Shouhua, et al. Cause analysis and process optimization of edge crack for 980 MPa cold rolled ultra high strength dual phase steel[J]. China Metallurgy, 2022, 32(9): 90-96. [4]岳重祥, 吴圣杰, 曹 垒, 等. 冷轧薄板边损边裂原因概述及实例分析[J]. 锻压技术, 2014, 39(11): 107-112. Yue Chongxiang, Wu Shengjie, Cao Lei, et al. Cause summary and case analysis of edge crack defects during the cold rolling process of thin steel sheet[J]. Forging and Stamping Technology, 2014, 39(11): 107-112. [5]罗晓宇, 乔及森, 赵文军, 等. 1235铝箔断带缺陷分析及成品力学性能[J]. 塑性工程学报, 2015, 22(6): 103-107. Luo Xiaoyu, Qiao Jisen, Zhao Wenjun, et al. Analysis of 1235 aluminum foil break belt defect and finished product mechanical property[J]. Journal of Plasticity Engineering, 2015, 22(6): 103-107. [6]王 畅, 于 洋, 王 林, 等. 含磷高强IF钢拉矫断带的原因及机制[J]. 钢铁, 2014, 49(5): 81-87. Wang Chang, Yu Yang, Wang Lin, et al. Research on the factors inducing strip fracture of high strength IF steel containing phosphorus during straightening process[J]. Iron and Steel, 2014, 49(5): 81-87. [7]王跃华, 宋进英, 魏英立, 等. 热轧窄带65Mn钢珠光体组织与性能的窄范围控制[J]. 钢铁钒钛, 2017, 38(2): 150-155. Wang Yuehua, Song Jinying, Wei Yingli, et al. Small range control of pearlite microstructure and properties of 65Mn hot rolled narrow strip[J]. Iron Steel Vanadium Titanium, 2017, 38(2): 150-155. [8]陈连生, 李 跃, 宋进英, 等. 55Mn冷轧带钢边裂的产生原因及冷轧控制措施[J]. 机械工程材料, 2017, 41(8): 31-34. Chen Liansheng, Li Yue, Song Jinying, et al. Reason for edge cracking of cold-rolled 55Mn strip steel and the cold-rolling control measures[J]. Materials for Mechanical Engineering, 2017, 41(8): 31-34. [9]魏扬华, 黄文静, 邢 军, 等. 热轧工艺对厚板板厚方向组织和力学性能均匀性的影响[J]. 材料热处理学报, 2023, 44(6): 100-108. Wei Yanghua, Huang Wenjing, Xing Jun, et al. Effect of hot rolling process on uniformity of microstructure and mechanical properties of thick plate in thickness direction[J]. Transactions of Materials and Heat Treatment, 2023, 44(6): 100-108. [10]钱 胜, 张文军, 林 威, 等. 热镀锌连退过程C翘机理及其预报模型[J]. 钢铁, 2021, 56(9): 88-95. Qian Sheng, Zhang Wenjun, Lin Wei, et al. Formation mechanism and prediction model for C-warping defect of strip steel in continuous annealing process of hot galvalume unit[J]. Iron and Steel, 2021, 56(9): 88-95. [11]吴春平, 袁勤攀, 肖 娟. 轧制温度对Q420钢组织和性能影响的研究[J]. 热加工工艺, 2023, 52(19): 88-90, 105. Wu Chunping, Yuan Qinpan, Xiao Juan. Study on effect of rolling temperature on microstructure and properties of Q420 steel[J]. Hot Working Technology, 2023, 52(19): 88-90, 105. [12]梁 宇, 余凌锋, 梁益龙. 珠光体钢微观组织与拉伸性能关系[J]. 材料热处理学报, 2013, 34(7): 73-77. Liang Yu, Yu Lingfeng, Liang Yilong. Relationship between microstructure and tensile properties of a pearlitic steel[J]. Transactions of Materials and Heat Treatment, 2013, 34(7): 73-77. [13]陈连生, 胡宝佳, 宋进英, 等. 冶金锯片用65Mn钢板球化退火后矫直断裂原因分析[J]. 热加工工艺, 2017, 46(24): 199-202. Chen Liansheng, Hu Baojia, Song Jinying, et al. Analysis of reasons for straightening fracture of 65Mn steel sheet after spheroidizing annealing in metallurgical saw blade[J]. Hot Working Technology, 2017, 46(24): 199-202. [14]卢 岳, 牛月鹏, 潘 进, 等. DH590冷轧板及镀锌板电阻点焊工艺窗口及点焊一致性的研究[J]. 热加工工艺, 2024, 53(3): 82-87. Lu Yue, Niu Yuepeng, Pan Jin, et al. Research on resistance spot welding process window and spot welding consistency of DH590 cold rolled sheet and its galvanized sheet[J]. Hot Working Technology, 2024, 53(3): 82-87. [15]钟明君, 王克鲁, 鲁世强, 等. 固溶时效对TC20钛合金显微组织和力学性能的影响[J]. 稀有金属材料与工程, 2021, 50(6): 2149-2154. Zhong Mingjun, Wang Kelu, Lu Shiqiang, et al. Effect of solution and aging on microstructure and mechanical properties of TC20 titanium alloy[J]. Rare Metal Materials and Engineering, 2021, 50(6): 2149-2154. [16]孙 璐, 李建英, 魏焕君, 等. 超高强马氏体钢开裂失效分析[J]. 金属热处理, 2023, 48(1): 261-266. Sun Lu, Li Jianying, Wei Huanjun, et al. Cracking failure analysis of ultra-high strength martensite steel[J]. Heat Treatment of Metals, 2023, 48(1): 261-266. [17]刘 威, 王 楠, 陈永楠, 等. 典型钛合金在简谐振动中的能量消耗和裂纹扩展行为[J]. 中国有色金属学报, 2022, 32(7): 1945-1954. Liu Wei, Wang Nan, Chen Yongnan, et al. Energy consumption and crack propagation behavior of typical titanium alloys during harmonic vibration[J]. The Chinese Journal of Nonferrous Metals, 2022, 32(7): 1945-1954. [18]秦永强, 袁 健, 罗来马, 等. 热处理对Y2O3掺杂WC-Co硬质合金显微组织及性能的影响[J]. 材料热处理学报, 2023, 44(4): 40-46. Qin Yongqiang, Yuan Jian, Luo Laima, et al. Effect of heat treatment on microstructure and mechanical properties of Y2O3 doped WC-Co cemented carbide[J]. Transactions of Materials and Heat Treatment, 2023, 44(4): 40-46. [19]刘 建, 李月丽. 钒氮微合金化对汽车用热轧钢板组织与力学性能的影响[J]. 塑性工程学报, 2022, 29(3): 150-156. Liu Jian, Li Yueli. Effect of V-N microalloying on microstructure and mechanical properties of hot-rolled steel plate for automobile[J]. Journal of Plasticity Engineering, 2022, 29(3): 150-156. [20]张明玉, 运新兵, 伏洪旺. BASCA热处理对TC10钛合金组织与断裂韧性的影响[J]. 材料导报, 2024, 38(7): 202-207. Zhang Mingyu, Yun Xinbing, Fu Hongwang. Effect of BASCA heat treatment on microstructure and fracture toughness of TC10 titanium alloy[J]. Materials Reports, 2024, 38(7): 202-207. [21]冯 力, 王 宁, 李邱达, 等. 微量元素C对AlCrCuFeMn高熵合金微观组织及力学性能的影响[J]. 中国有色金属学报, 2023, 33(11): 3767-3777. Feng Li, Wang Ning, Li Qiuda, et al. Effect of trace element C on microstructure and mechanical properties of AlCrCuFeMn high entropy alloy[J]. The Chinese Journal of Nonferrous Metals, 2023, 33(11): 3767-3777. [22]张慧书, 李吉航, 战东平, 等. 稀土La对Ferrium S53超高强度钢组织和性能的影响[J]. 钢铁研究学报, 2023, 35(12): 1569-1578. Zhang Huishu, Li Jihang, Zhan Dongping, et al. Effect of rare earth La on microstructure and properties of Ferrium S53 ultra high strength steel[J]. Journal of Iron and Steel Research, 2023, 35(12): 1569-1578. [23]莫文锋. 珠光体片间距的热力学控制及其对钢力学性能的影响[J]. 钢铁钒钛, 2021, 42(5): 175-179. Mo Wenfeng. Thermodynamic control of pearlite lamellar sheet spacing and its effect on mechanical properties of steel[J]. Iron Steel Vanadium Titanium, 2021, 42(5): 175-179. [24]王 燕, 方 峰, 王 雷, 等. 冷拔珠光体钢丝渗碳体微观结构[J]. 材料热处理学报, 2010, 31(5): 92-95. Wang Yan, Fang Feng, Wang Lei, et al. Microstructure evolution of cementite in cold drawn pearlitic steel wires[J]. Transactions of Materials and Heat Treatment, 2010, 31(5): 92-95. [25]范振霞, 赵昊乾, 秦树超. H82A硬线钢面缩率偏低的分析[J]. 热加工工艺, 2021, 50(17): 148-151. Fan Zhenxia, Zhao Haoqian, Qin Shuchao. Analysis of low area reduction of H82A hard wire steel[J]. Hot Working Technology, 2021, 50(17): 148-151. [26]姚三成, 宫彦华, 赵 海, 等. 加热温度对钒微合金中碳钢组织及性能的影响[J]. 材料热处理学报, 2020, 41(2): 67-74. Yao Sancheng, Gong Yanhua, Zhao Hai, et al. Effect of heating temperature on microstructure and properties of vanadium microalloyed medium carbon steel[J]. Transactions of Materials and Heat Treatment, 2020, 41(2): 67-74. [27]魏泽民, 梁 宇, 梁益龙, 等. 高碳钢中珠光体片层与先共析铁素体对断裂韧性的影响[J]. 材料热处理学报, 2016, 37(1): 126-132. Wei Zemin, Liang Yu, Liang Yilong, et al. Effect of interlamellar pearlite spacing and pro-eutectoid ferrite on fracture toughness of high-carbon steel[J]. Transactions of Materials and Heat Treatment, 2016, 37(1): 126-132. [28]梁 宇, 向 嵩, 梁益龙, 等. 原奥氏体晶粒尺寸对珠光体钢组织及韧性的影响[J]. 材料导报, 2017, 31(2): 77-81. Liang Yu, Xiang Song, Liang Yilong, et al. Effect of prior austenite grain size on microstructure and toughness of pearlitic steel[J]. Materials Reports, 2017, 31(2): 77-81. [29]周 云, 杨晓伟, 陈焕德, 等. 加热温度对600 MPa级高强钢筋组织及性能的影响[J]. 钢铁, 2020, 55(1): 101-107. Zhou Yun, Yang Xiaowei, Chen Huande, et al. Effect of heating temperature on microstructure and properties of 600 MPa grade high strength steel rebars[J]. Iron and Steel, 2020, 55(1): 101-107. [30]万志健, 赵 海, 刘学华, 等. 钒对车轮钢组织及力学性能的影响[J]. 钢铁, 2023, 58(5): 104-111. Wan Zhijian, Zhao Hai, Liu Xuehua, et al. Effect of V on microstructure and mechanical properties of wheel steel[J]. Iron and Steel, 2023, 58(5): 104-111. [31]鲁修宇, 刘 静, 张云燕, 等. 控冷工艺对高强桥索盘条组织和性能的影响[J]. 热加工工艺, 2019, 48(7): 23-27. Lu Xiuyu, Liu Jing, Zhang Yunyan, et al. Effect of controlled cooling process on microstructure and properties of high strength bridge cable wire rod[J]. Hot Working Technology, 2019, 48(7): 23-27. [32]霍雄勃, 党淑娥, 赵家兴, 等. 热处理工艺对ER7车轮钢力学性能的影响[J]. 金属热处理, 2021, 46(3): 51-55. Huo Xiongbo, Dang Shue, Zhao Jiaxing, et al. Effect of heat treatment process on mechanical properties of ER7 wheel steel[J]. Heat Treatment of Metals, 2021, 46(3): 51-55. [33]赵建宁, 毛卫民, 王庆贤, 等. 热轧过程对T7钢帘线组织与性能的影响[J]. 金属热处理, 2008, 33(12): 69-72. Zhao Jianning, Mao Weimin, Wang Qingxian, et al. Influence of hot rolling process on microstructure and mechanical properties of T7 steel cord[J]. Heat Treatment of Metals, 2008, 33(12): 69-72. |