Effect of solution treatment on properties of DSS2205 laser weld seam

Wang Weidong1,2, Bi Zongyue1,2, Xian Linyun1,2, Wang Haitao1,2, Li Xiaolong1,2, Liu Yudong1,2, Yu Chenyang1,2, Xu Xueli3   

  1. 1. Chinese National Engineering Research Center for Petroleum and Natural Gas Tubular Goods, Baoji Shaanxi 721008, China;
    2. Baoji Petroleum Steel Pipe Co., Ltd., Baoji Shaanxi 721008, China;
    3. School of Materials Science and Engineering, Xi'an Shiyou University, Xi'an Shaanxi 710065, China
  • Received:2020-06-02 Online:2020-12-25 Published:2021-01-14

Abstract: Aiming at the problem of disproportionate of ferrite and austenite of duplex stainless steel weld seam after laser welding, the DSS2205 laser weld seam was solution treated at different temperatures and time through the Gleeble-1300 thermal simulation tester. The results show that under different solid solution conditions, the austenite morphology and the two phase ratios change greatly. With the increase of temperature and holding time, the alloying elements fully diffuse and migrate in the two phases, and the austenite grain gradually grows, the content first increases and then decreases. After solution treated at 1050 ℃ for 5 min, the microstructure of the specimen is uniform, the proper proportion of ferrite and austenite phase can be obtained, the hardness gradient of weld seam is uniform, and the impact property becomes the best.

Key words: solution treatment, DSS2205, weld seam, microstructure, properties