Heat Treatment of Metals ›› 2022, Vol. 47 ›› Issue (11): 178-183.DOI: 10.13251/j.issn.0254-6051.2022.11.032

• MATERIALS RESEARCH • Previous Articles     Next Articles

Effect of Ni on microstructure and mechanical properties of 30CrMnSi2 steel

Ma Jinwei1, An Shengli1, Jia Li2, Fu Xueyi3, Xue Rui2, Gao Zhanyong1   

  1. 1. College of Materials and Metallurgy, Inner Mongolia University of Science and Technology, Baotou Inner Mongolia 014010, China;
    2. Ordos City Shendongtianlong Mining Machine Co., Ltd., Ordos Inner Mongolia 017200, China;
    3. Baogang Incorporated Company, Baotou Inner Mongolia 014010, China
  • Received:2022-05-20 Revised:2022-08-24 Online:2022-11-25 Published:2023-01-04

Abstract: Microstructure and properties of 30CrMnSi2 steel with different Ni contents after tempering at low temperature were studied. The results show that the microstructure of the tested steel consists of tempered lath martensite and M/A islands. With the increase of Ni content, the M/A islands are significantly refined, and changing from islands to elongated strips. The impact fracture is ductile fracture, with the increase of Ni content, the ductile area of the fracture increases, the equiaxial dimple deepens, the number of dimples increases, and the impact absorbed energy increases. When the Ni content is greater than 1.0%, the increasing trend of impact absorbed energy decreases. The tested steel with 1.0%Ni has the highest strength, good toughness and plasticity, and the best comprehensive properties.

Key words: 30CrMnSi2 steel, Ni content, lath martensite, microstructure, mechanical properties