HTM ›› 2014, Vol. 39 ›› Issue (3): 108-112.DOI: 10.13251/j.issn.0254-6051.2014.03.000

Previous Articles     Next Articles

Phase and properties of HA/TiO2 composite coating deposited by Hydrothermal-electrochemical deposition

  

  1. School of Mechanical Engineering, University of Shanghai for Science and Technology; School of Materials Science and Engineering, University of Shanghai for Science and Technology
  • Online:2014-03-25 Published:2014-04-28

Key words: HA/TiO2 composite coating, hydrothermal electrochemical deposition, phase, bonding strength, biological activity

CLC Number: