HTM ›› 2014, Vol. 39 ›› Issue (5): 150-153.DOI: 10.13251/j.issn.0254-6051.2014.05.039

Previous Articles     Next Articles

Failure analysis of hydrocylinder

  

  1. School of Materials Science and Engineering, China University of Mining and Technology; Xuzhou XuGong Hydraulic Component Co., Ltd.
  • Online:2014-05-25 Published:2014-05-28

Key words:  welding cooling rate, martensite, brittleness, early fatigue cracks