[1] |
Meng Xiangjun, Shen Ying, Zhang Shaoyu, Xu Hongliang, Wang Yang, Liu Xiubo.
Microstructure and tribological properties of laser clad Co-Ti3SiC2 composite coating on Ti6Al4V alloy
[J]. Heat Treatment of Metals, 2021, 46(12): 199-203.
|
[2] |
Deng Pengfei, Zuo Linchun, Chen Xingwei, Xiong Wei, Liu Yan, Liao Conglai, Li Zhi.
Oxidation resistance of hot-dip aluminized coating on cast K438 superalloy
[J]. Heat Treatment of Metals, 2021, 46(11): 207-212.
|
[3] |
Tan Haibo, Shi Zhoulong, Zhang Shumei, Zhu Juanjuan.
Effect of β annealing parameter on microstructure and properties of Ti6Al4V titanium alloy
[J]. Heat Treatment of Metals, 2021, 46(1): 209-213.
|
[4] |
Xiao Meili, Zan Lin, Ke Linda, Deng Zhujun, Lai Caifang, Sun Jingli.
Effect of annealing process on microstructure and room temperature mechanical properties of selective laser melted Ti6Al4V alloy
[J]. Heat Treatment of Metals, 2020, 45(8): 108-112.
|
[5] |
Zhao Jiefu, Chu Longsheng, Liu Jun, Gao Peng.
Effect of micro-arc oxidation treatment on adhesion properties between stainless steel and epoxy resin
[J]. HTM, 2020, 45(3): 92-96.
|
[6] |
Zheng Nianqing1,Yang Jin2,Wang Jianguo1,Zhang Heng2,Fan Zhishan1,Zhang Peng1,Feng Ran1,Lai Yunjin1.
Effect of microstructure of Ti6Al4V alloy on ultrasonic wave velocity
[J]. HTM, 2015, 40(8): 59-63.
|
[7] |
Yan Jikang 1,2, Tang Wanxia1,2, Ni Erxin1,2, Wu Yunfeng 1, Fang Shuming 1, Yang Gang 1.
Effect of oxidation time on structure and corrosion resistance property of micro-arc oxidation film on Ti6Al4V
[J]. HTM, 2015, 40(10): 86-91.
|