[1] |
Ji Guoqiang, Ge Guiming, Yu Lijuan, Zhong Jizhi.
Analysis on cracking of 50CrV4 steel washer
[J]. Heat Treatment of Metals, 2021, 46(7): 254-257.
|
[2] |
Yang Yu, Wang Yinghai, Zhang Jifu, Ma Xiaojun, Xu Lijia, Ren Junwei.
Formation cause analysis of electroplating mildew spot on 45Mn steel part surface
[J]. Heat Treatment of Metals, 2021, 46(4): 220-223.
|
[3] |
Zhang Jiawen, Fu Tianliang, Wu Hao, Wang Zhaodong.
Cause analysis on quenching cracking of 40CrNiMo7 steel forged shaft
[J]. Heat Treatment of Metals, 2021, 46(2): 213-217.
|
[4] |
Li Mingyang, Wang Fuming, Li Ming, Gong Shuo.
Effect of inclusions on fatigue life of engineering machinery structural steel Q345FCA
[J]. Heat Treatment of Metals, 2020, 45(8): 7-11.
|
[5] |
Chen Wei, Wang Yong, Han Jian.
Cause analysis on spalling of working roll during cold rolling
[J]. Heat Treatment of Metals, 2020, 45(6): 232-235.
|
[6] |
Li Bingbing, Chen Haitao, Lang Yuping, Qu Huapeng, Feng Hanqiu, Tian Zhiling, Chen Qingming.
Solution behavior of copper-containing super austenitic stainless steel
[J]. Heat Treatment of Metals, 2020, 45(11): 68-72.
|
[7] |
Yu Chunming, Zhang Jiming.
Failure analysis and improvement of bending cracking of low alloy Q345B steel treated by ultra-fast cooling process
[J]. HTM, 2020, 45(1): 239-244.
|
[8] |
Zhang Chi1, Zhang Shuangjie1, Feng Jie1, Yang Shufeng2, Dai Yongjuan1.
Effect of sulfide inclusions on pitting behavior of steel
[J]. HTM, 2016, 41(9): 62-65.
|
[9] |
Tian Yaqiang, Li Ran, Song Jinying, Zhang Ronghua, Zheng Xiaoping, Chen Liansheng.
Analysis on peeling defects of cold-rolled sheet and its influencing factor
[J]. HTM, 2016, 41(9): 174-178.
|
[10] |
Lei Xiaojuan, Hou Ting.
Failure analysis of transmission middle shaft
[J]. HTM, 2016, 41(5): 203-205.
|
[11] |
Qin Huaipeng1, 2, Chen Haitao2, Lang Yuping2, Chen Qingming1.
Thermodynamic calculation of inclusions formation and morphology analysis of 439 ferritic stainless steel
[J]. HTM, 2015, 40(6): 176-182.
|
[12] |
Hu Ping, Zhang Chuanguo, Zheng Lei.
Effects of cooling process and chemical composition on microstructure and properties of X100 pipeline steel
[J]. HTM, 2015, 40(3): 140-146.
|
[13] |
Liu Cheng1,Zhao Bin1,Zhao Zhenbo2,Liu Yunxu3.
Role of carbon in super bainite steels
[J]. HTM, 2015, 40(2): 1-7.
|
[14] |
Li Hongke, Song Bo, Wang Liyong, Yang Yuhou, Chen Maochuan.
Effect of austenitizing temperature on microstructure of La deoxidized steel
[J]. HTM, 2014, 39(7): 1-6.
|
[15] |
Qi Guoquan, Li Xunji, Qiang Yuan, Wang Fushan.
Failure analysis of P110 casing crack in hydrostatic proof test
[J]. HTM, 2014, 39(7): 166-169.
|