Annealing process of SAl 4047 Al-Si alloy solder?wire during drawing

  

  1. 1. Sichuan University of Science and Engineering; 2. Sichuan Atlantic Welding Consumables Co., Ltd.
  • Online:2016-08-25 Published:2016-09-02

Key words: SAl 4047 aluminum alloy wire, annealing process, microstructure, mechanical properties, drawing property